Water quality has a major impact on hydro dipping services. One recurring problem with this method is the presence of a slimy film even after rinsing. This has a lot to do with the quality of the water and the way the hydrodipping tank is maintained. In this blog, Solera Metal Fabrication, a major fabrication facility in Brampton, Ontario, offering hydro dipping services, metal laser cutting and more, explores these concepts.
What Is The Importance Of Water Quality For Hydrographic Dipping?
The cause of sliminess in water used in hydrographic dipping is the presence of dissolved minerals in it. The most common minerals include calcium and magnesium. Also known as hard water, using this untreated water can cause inconsistent results when rinsing the hydrographic film, which is the main cause of sliminess.
The best way to remove this hardness is by using a water softener along with a filtration system to ensure water purity.
What Tank Maintenance Practices Can Help Improve The Results Of Hydrographic Dipping?
Clean The Tank
Cleaning the tank is mandatory to ensure consistent results during hydrographic dipping. This involves multiple steps, such as removing floating debris from the surface of the water, wiping tank walls and draining on a regular schedule.
Maintain Water Temperature
Make sure that the temperature of the water is not fluctuating a lot. Changing water temperatures can negatively impact the overall adhesion during the dipping process.
Avoid Contamination
The rinsing areas have to be kept clean and pristine. Make sure that it is free from any debris and contaminants.
Ensure Thorough Rinsing
When rinsing, make sure that the slimy texture is completely gone. This is a great indicator that rinsing is successful.
Conclusion
In closing, taking water quality and tank conditions into account goes a long way towards ensuring proper film adherence during hydrographic dipping.
Want custom designs and prints for your project? Solera Metal Fabrication is here to assist. Apart from our custom hydro dipping services, we also offer sheet metal laser cutting, tube laser cutting services, powder coating services, and much more. Contact us at 905-457-4777 to learn more about end-to-end fabrication services.
FAQs:
How durable is the finish during hydro dipping?
The finish after hydro dipping is extremely durable, aesthetic, scratch- and weather-resistant.
Is there an ideal water temperature for hydrographic dipping?
There is a preferable temperature range for hydrographic dipping, which is around 27-32 degrees Celsius.